ACRYLIC COATING


Preparation and application procedure

PREPARATION
Procedure:

  • Rinse the surface well with a pressure washer.
  • Apply TexNov Surface Preparer according to the dilution table below.
  • Brush the surface vigorously and leave for 15 minutes.
  • Rinse the surface thoroughly with a pressure washer.
  • Let the surface dry for 48 hours in good weather before applying the finishing coat.

FINISH COATING
Procedure :

  • Apply 2 coats ofTexNov Acrylic Coating using a brush or roller with 10 mm bristles.
  • Leave 24 hours between each coat.
  • Allow the surface to dry for 24 hours before applying the sealant.
SEALANT
After having done the surface preparation and the application of the coating (if necessary)…

Procedure :

  • Apply 2 coats of TexNov WRS-40 waterproofing sealer to waterproof the surface. Use a brush, roller with 10 mm bristles or sprayer.
  • Allow 24 hours drying time between coats.
  • Let the surface dry for 24 hours.

MAINTENANCE :

Clean the surface with TexNov Surface Preparer by diluting 9 parts water to 1 part product. Let dry and add a coat of WRS-40 Sealer every 5 years or as needed, which should allow you to keep your surface in good condition.